Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
Westlake Plastics PEEK PEEK is a high performance semi-crystalline thermoplastic. PEEK characteristics include high temperature performance, excellent wear properties, superior chemical resistance and outstanding toughne.. |
|||
Tensile Modulus | 3.59 GPa @Temperature 150 °C |
520 ksi @Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
ScanTube PEEK Tubing Information provided by ScanTube, Inc. |