Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 34.483 GPa | 5001.3 ksi | ASTM D-638 |
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC.. |