Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.40 GPa | 493 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 OB Polyamide 6, Optically Brightened FeaturesPA 6 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and tensile modulus in comparison with the basic type. The microcrystal.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Aquanyl Nylon 612 Copolymer Aquanyl is a copolymer of Nylon 6 and Nylon 12 produced via the anionic polymerization process using the monomer's Caprolactam and Laurinlactam. It has reduced water absorption, improved stability a.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific) PC/ABS with high stiffness and impact performance |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | |
Radici Radilon® CS 35FL (dry) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP R1000S PA 66 LNP COLORCOMP* R1000S is an unfilled Nylon 66. Added features of this material is: Heat Stabilized. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP R1000SU PA 66 LNP COLORCOMP* R1000SU is an unfilled Nylon 66 resin. Added features include: Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ASTM D638 |
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | |
LATI Latimass 66-04 D009 PBT Specific density compound based on Polybutylene Terephthalate (PBT). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
Polyram RamTal PMH2022 Polyacetal Homopolymer for Injection Molding General purpose polyacetal homopolymer for injection molding applications, MFI 22.Information provided by Polyram. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ASTM-D790 |
Polyram RamTough PZ322G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
DSM Akulon® S223-F Nylon 66 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the health.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PX06020 PA6, Flame Retardant, Injection Molded Starflam PX06020 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
CENTROPLAST CENTRO HPM Polyetherimide This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |