Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.33 GPa | 483 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 3.33 GPa | 483 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Tensile Modulus | 3.33 GPa | 483 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant. |