Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.28 GPa | 476 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 3.28 GPa | 476 ksi | 1 mm/min |
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP.. |
|||
Tensile Modulus | 3.28 GPa | 476 ksi | 1 mm/min |
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol.. |
|||
Tensile Modulus | 3.28 GPa | 476 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 3.28 GPa | 476 ksi | ASTM Data |
Dow Tyril® 100 SAN Data provided by Dow Chemical. |