Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.307 GPa | 44.5 ksi | 1 mm/min |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |