Polymer Property : Tensile Modulus = 41500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 286 GPa
41500 ksi
Toho Tenax Besfight® G40-800 12K IMA5C EP03 Continuous Filament Carbon Fiber
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho..
Tensile Modulus 286 GPa
41500 ksi
Toho Tenax Besfight® G40-800 24K IMA5C EP03 Continuous Filament Carbon Fiber
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho..
Tensile Modulus 286 GPa
41500 ksi
Toho Tenax Besfight® G40-800 6K IMA-5C EP03 Continuous Filament Carbon Fiber
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho..