Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.71 GPa | 393 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | ASTM D638 |
Nilit Polynil® P230 High Viscosity Nylon 66 Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various.. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | ASTM D638 |
Nilit Polynil® P240 High Viscosity Nylon 66 Description: Polynil P240 is a high viscosity NYLON 66 (Viscosity number 290 cm³/gr) that was developed for rod and slab extrusion. It has a high melt stability and a low gel content.Key characteri.. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | Storage |
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in.. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |
|||
Tensile Modulus | 2.71 GPa | 393 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific) LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |