Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 26.88 GPa | 3899 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |