Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 26.2 GPa @Temperature 23.9 °C |
3800 ksi @Temperature 75.0 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Tensile Modulus | 26.2 GPa @Temperature 23.9 °C |
3800 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F 2kpsi; ASTM D638 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Tensile Modulus | 26.2 GPa @Temperature 23.9 °C |
3800 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-670F Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670F is a versatile, non-styrenated/low VOC polyester resin. P670F is used in a wide variety of applications including tooling and aircraft structures.Key Features and Benefits:Non-styre.. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | Prepreg, RT, Dry |
Renegade Materials Corporation RM-5003 Cyanate Ester Prepreg 4581 Quartz Fabric Low dielectric and loss, high performance prepreg. 350°F Cure Developed with consistent handling and superior performance Designed for demanding electrical, radome and antennae applications Del.. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA.. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp JX89569 PES LNP THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding. |
|||
Tensile Modulus | 26.2 GPa | 3800 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp JX89569 PES (Asia Pacific) LNP* THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |