Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.61 GPa | 379 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific) High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East) High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 1mm/min |
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | |
Abatron AboCast 8103-25 High-Performance Dielectric Epoxy AboCast 8103-25 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines o.. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | ASTM D-638 |
Axiall Suprel® SVA 9301 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li.. |
|||
Tensile Modulus | 2.61 GPa | 379 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |