Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.60 GPa | 377 ksi | |
Plastcom SLOVAMID 66 MI PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasalac 3P-H9000B ABS/PC Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | |
Radici Radilon® S CP400 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | |
Ineos ABS Lustran® QE 1455, Injection Grade
(discontinued **) Injection molding grade, increased heat resistance, medium gloss.Applications: Automotive: interior parts.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renam.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | |
Ineos ABS Lustran® H950 Very high heat resistance,,Property data per ISO test methods. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-8960 60% Barium-Sulfate Filled Polypropylene Block-Copolymer INNOPOL® CS 2-8960 is a 60% Barium-sulfate filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8960 is developed for.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP CF 2200 000000 PBT+PC PBT+PC, non-reinforced, injection molding, flame retardant, impact modified, low tendency to warp |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1mm/min; ISO 527-2/1A |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
American Polymers 370 Polystyrene, High Heat Data provided by American Polymers, Inc. A high heat polystyrene produced in pellet form. It has excellent strength and clarity as well as fast set-up properties. Used in the manufacture of toys,.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Bayblend® FR3200 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
Covestro Makrolon® 1899* Polycarbonate, Impact Grade Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DSM Arnite® T06 200 SNF PBT (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min |
Polimeri Europa KOBLEND PCA 51 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 90°C Main application field.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min |
Polimeri Europa KOBLEND PCA 53 PC+ABS