Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.598 GPa | 376.8 ksi | ASTM D638 |
SABIC PS 126 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 125 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and hi.. |