Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.41 GPa | 350 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG38U ABS High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® X37 ABS ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS PC+ABS. Electroplateable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SY-03CF/000 Polystyrene - High Impact (HIPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1301-10 Polycarbonate Resin Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Spartech UltraTuf SG Polycarbonate Sheet Description: Polycarbonate SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 2 in/min; ASTM D638 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-15 Polycarbonate EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM Data |
Styron Magnum™ 9015 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6) Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a vari.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6) Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo.. |
|||
Tensile Modulus | 2.41 GPa @Temperature 23.0 °C |
350 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |