Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.34 GPa | 340 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-000/8T Acetal-Copolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Star Plastics PC20NBR Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 2 in/min; ASTM D638 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 2 in/min; ASTM D638 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 2 in/min; ASTM D638 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Total PSI 740 Polystyrene Polystyrene 740 is an impact polystyrene designed for extrusion and injection molding. It is especially suitable for extrusion thermoforming applications requiring high glass and high stiffness, suc.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU) TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated
(discontinued Description/Features:Glass Bead FilledPTFE/Silicone LubricatedInformation provided by PolyOne Corporation. |