Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 23.0 GPa | 3340 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-30LCF/002 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | Conditioned; ISO 527-2 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ISO 527 |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Conditioned) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ISO 527 |
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass 60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ISO 527-1 |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45 Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon .. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **) PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Tensile Modulus | 23.0 GPa | 3340 ksi | ASTM D638 |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |