Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.25 GPa | 326 ksi | |
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ASTM D638 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ASTM D638 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
LG Chemical HI-121 ABS, High Impact Feature: Injection Molding, Well Balanced Mechanical PropertiesApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information Provided by LG Chem |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 640 Injection Molding Grade Lustran® ABS 640 has high impact strength and is injection molding grade. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 650 Injection Molding Grade Lustran® ABS 650 has high impact strength, high flow, and is injection molding grade. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 970 Lustran® ABS 970 has high impact strength and good paintability. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
Styrolution Novodur® 4115 ABS Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527-1/-2 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade Information provided by Eurotec® |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1mm/min; ISO 527 |
Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy PC/ABS polymer alloy general grade developed for automobile parts use. It has high heat resistance, impact strength, light resistance and fluidity, particularly, the high impact strength in a wide r.. |
|||
Tensile Modulus | 2.25 GPa @Temperature -70.0 °C |
326 ksi @Temperature -94.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min |
Polimeri Europa SINKRAL G323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-20 General purpose injection moulding grade. Main properties are: good impact resistance high flow e.. |
|||
Tensile Modulus | 2.25 GPa | 326 ksi | |
Henkel Hysol EA 956 Paste Adhesive System Very low viscosity, cures at room temperatureDesigned for wet lay-up repairApplications: Structural Repair Low Viscosity Wet Lay-Up |