Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.206 GPa | 320.0 ksi | ASTM D638 |
Resirene Resirene® 2270 High Impact Polystyrene Features:Medium FlowGood GlossFDA Rating: 21 CFR 177.1640High ProductivityApplications:Extrusion/ ThermoformingInjectionDiskettesPen BarrelsInformation provided by US distributor Calsak Corporation... |
|||
Tensile Modulus | 2.206 GPa | 320.0 ksi | ASTM D638 |
Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA) Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office pr.. |