Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 21.63 GPa | 3137 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed) |
|||
Tensile Modulus | 21.63 GPa | 3137 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. |