Mechanical Properties Metric English Comments
Tensile Modulus 216 GPa
31300 ksi
Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
Tensile Modulus 216 GPa
31300 ksi
Toho Tenax Besfight® MC Type II (3000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
Tensile Modulus 216 GPa
31300 ksi
Toho Tenax Besfight® MC Type II (6000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..