Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.14 GPa | 310 ksi | |
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 142-EX is a medium viscosity, sag resistant epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance is desired. Thi.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp FFL21 PE (Asia Pacific) LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech CamAlloy /ABS Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech SP-9013 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech SP-9020 Premium ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D 638 |
Styrolution PS 6200/6201 HIPS Excellent toughnessDesigned for deep draw thermoformingUSP Class VI certifiedInformation provided by Styrolution |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D 638 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |