Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.05 GPa | 297 ksi | |
Plastcom SLOVALEN PC 93 T 20 PP, 20% mineral filling, UV stabilization FeaturesModified PP for injection moulding with the content of 20 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527-2 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527-2 |
Total PSI 4440(EU) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ASTM D 638 |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 902 UR POM Copolymer unreinforced, impact modified POM-IInformation provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe) Special tough to rigid grade with very good gloss for all types of housings.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 2.05 GPa | 297 ksi | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |