Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D-638 |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Tensile Modulus | >= 20.0 GPa | >= 2900 ksi | ISO 527-1,2 |
Qualchem Danamid AFCF-30 Polyamide 66, 30% Carbon Fiber Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 20.0 GPa @Temperature 23.0 °C |
2900 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ASTM D-638 |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | Conditioned; ISO 527-2 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AE006 ABS LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
Tensile Modulus | 20.0 - 23.0 GPa | 2900 - 3340 ksi | ISO 527 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Vyncolit X640 Resole Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Tensile Modulus | 20.0 - 30.0 GPa | 2900 - 4350 ksi | Parallel to Plane |
Goodfellow Carbon-Carbon Composite Carbon Fiber - Carbon MatrixInformation provided by Goodfellow. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | 0º |
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 600 g/m2 Information provided by HexCel |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-1/-2 |
DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527 |
Eurotec® Tecomid® NA40 KC50 BK111 PA6.6, 50% glass/carbon fiber reinforced, black Information provided by Eurotec® |
|||
Tensile Modulus | 20.0 GPa | 2900 ksi | ISO 527-1 |
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |