Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.93 GPa | 280 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D2000P PC (Asia Pacific) LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D 638 |
Shakespeare Isocorâ„¢ CU145SI Nylon 6/66 Isocorâ„¢ CU145SI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balan.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Spartech GELOY SP-6730 Weatherable Sheet Description: Weatherable SheetGeloy is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Test |
Styrolution Terblend® N NM-11 ABS/PA6 (Dry) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Test |
Styrolution Terblend® N NMX04 ABS/PA6 (Dry) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D882 |
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compli.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
American Polymers API 545 Polystyrene API 545 is a high impact, high heat resistant grade of impact modified polystyrene. This material features fast set-up as well as easy colorability.Applications: API 545 is suggested for heavy part.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Americas Styrenics STYRON® 404 High Impact Polystyrene Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D-638 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
American Polymers API 425 Polystyrene API 425 is a medium impact grade of polystyrene for injection molding. API 425 has good gloss, easy flow and fast cycling properties.Applications: API 425 is widely used in cosmetic packaging, food.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific) LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics PREVEX W20 PPE+PS Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |