Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 19.0 - 21.0 GPa | 2760 - 3050 ksi | ISO 527 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit TX10916 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H SST black 9288 PA12-GF65 Product description: Grilamid LV-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the f.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA) 55% Glass Reinforced PPA High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30 Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiff.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Barlog Plastics KEBATRON C1065X1 PPS, cross-linked, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1 |
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ASTM D638 |
LNP Lubricomp® OCL-4534 EM Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discont Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |