Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.621 GPa | 2700.8 ksi | ASTM D-638 |
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiC.. |