Polymer Property : Tensile Modulus = 2670 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 18.4 GPa
2670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include : Electrically Conductive.
Tensile Modulus 18.4 GPa
2670 ksi
ASTM D638
Unitika RUN35-C25 Weather resistant PA6, Dry
Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd.
Tensile Modulus 18.4 GPa
2670 ksi
1mm/min; ISO 527
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.