Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.16 GPa | 2634 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12 LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive. |