Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | MD; ASTM D882-A |
Borealis FG5190 Linear Low Density Polyethylene FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D638 |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D638 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D638 |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D638 |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D638 |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D638 |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | 1 mm/min |
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Tensile Modulus | 0.170 GPa | 24.7 ksi | ASTM D882 |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |