Polymer Property : Tensile Modulus = 2329 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 16.06 GPa
2329 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA 12 (Asia Pacific)
LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 16.06 GPa
2329 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA12
LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing 50% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant.