Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | chs 2 in/min; ASTM D638 |
Network Polymers NPS 90-0802 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | TM R050-36 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PE-30MC-20TC/000 High Density Polyethylene (HDPE), Talc Filled
(discontinued **) Description/Features:Mica FilledTalc FilledInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | |
Saint-Gobain Rulon® 125 Bearing/Seal PTFE Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Tensile Modulus | 1.58 GPa | 230 ksi | Storage |
Epoxy Technology EPO-TEK® B9021 Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Tensile Modulus | 1.58 GPa @Temperature 30.0 °C |
230 ksi @Temperature 86.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
American Polymers API 550 Polystyrene API 550 is a high impact grade of polystyrene. It is characterized by good impact and processability.Applications: API 550 is widely used in housewares, toys, containers, appliance parts, speaker h.. |