Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.4 GPa | 2230 ksi | |
LATI Latiohm 62-03 PD01 G/20 PPA, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Tensile Modulus | 15.4 GPa @Temperature 100 °C |
2230 ksi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F10 Nylon 6, 50% Glass Fiber SAXAMID 126F10 is a polyamide 6 injection-molding-grade reinforced with 50% glass fibers.Information provided by SAX Polymers |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | ASTM D638 |
Plenco 6015 Phenolic, Briquette, Injection Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar. |
|||
Tensile Modulus | 15.4 GPa | 2230 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 15.4 GPa @Temperature 100 °C |
2230 ksi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |