Tensile Modulus 15.21 GPa
2206 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6
LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber.
Tensile Modulus 15.21 GPa
2206 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific)
LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber.