Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.8 GPa | 2140 ksi | Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content. |
Fibre Glast Saf-T-Poxy 2410 / 2184 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |