Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.5 GPa | 2100 ksi | |
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | |
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 14.48 GPa | 2100 ksi | ASTM D-638 |
PlastiComp Complet® LCF10/LGF30 - PP Polypropylene, 40% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1,-2 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | |
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFN18 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18 is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. |
|||
Tensile Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UX06028 PPA (Europe-Africa-Middle East) LNP * THERMOCOMP* UX06028 is a compund based on Polyphthalamide resin, containing Glass Fiber. Added features include Mold Release. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TW242FM10 PA46-(GF+MF)50 50% Glass/Mineral Reinforced, Heat Stabilized |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1 |
Barlog Plastics KEBAFLOW MF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |