Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.46 GPa | 2097 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF) LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant. |