Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min |
Polimeri Europa SINKRAL B813 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, providing very high impact resistance, even at low temperatures. Used as.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 238 Black 21 N PA66, Conditioned Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Tensile Modulus | 1.40 - 2.20 GPa @Thickness 2.00 mm |
203 - 319 ksi @Thickness 0.0787 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP C1000XXP PS (Europe-Africa-Middle East) LNP* THERMOCOMP* C1000XXP is a compound based on Polystyrene resin. Added features include: High Impact. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1mm/min; ISO 527-2 |
Borealis BJ360MO Polypropylene Copolymer BJ360MO is a heterophasic copolymer. This grade provides unique combination of very high melt flow rate, high impact strength and stiffness. and is designed for high-speed injection molding and cont.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1mm/min; ISO 527-2 |
Borealis HB600TF Polypropylene HB600TF is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master batch without .. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Total PPH 3051 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3051 is homopolymer.ApplicationATOFINA Polypropylene PPH 3051 is intended for the extrusion of flat bioriented films for food packaging or high strength adhesive tapes. Inf.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Total PPH 3150 Polypropylene, Homopolymer Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films .. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 L PA12 Product Description: Grilamid L 20 L is a medium viscosity Polyamide 12 (PA12) extrusion type. It is UV and heat stabilized. Its main features are: High surface quality Very good UV and heat resista.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2/1 |
ExxonMobil PP1014H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | Storage |
Epoxy Technology EPO-TEK® B9021-1 Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHSA NC010 is a heat stabilized lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, Conditioned Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Conditioned (2.5% Moisture) Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
BASF Novolen® 1102 K Polypropylene Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |