Tensile Modulus 13.85 GPa
2009 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 (Asia Pacific)
LNP* Thermocomp* RF0069SZ is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Tensile Modulus 13.85 GPa
2009 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV008S PA 66
LNP* VERTON* RV008S is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.
Tensile Modulus 13.85 GPa
2009 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV008S PA 66 (Asia Pacific)
LNP* Verton* RV008S is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.