Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 138 GPa | 20000 ksi | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S(HT) Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-85(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
PSM Industries Pacific Sintered Metals Nickel Iron FN-250-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0200-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S(HT) Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0208-130HTInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 138 GPa | 20000 ksi | ASTM D3039 |
Greene Tweed WR™ 525 PEEK, Carbon Filled WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | 0°; RT |
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, Annealed Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, Extra Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | ASTM E8 |
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for .. |
|||
Tensile Modulus | 138 GPa | 20000 ksi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-35Information Provided by Pacific Sintered Metals, a division.. |