Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.6 GPa @Temperature 23.0 °C |
1970 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Tensile Modulus | 13.6 GPa | 1970 ksi | |
LATI Latiohm 57-05 PD01 G/15 PPA, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Tensile Modulus | 13.6 GPa | 1970 ksi | 1mm/min; ISO 527 |
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Tensile Modulus | 13.6 GPa | 1970 ksi | ISO 527-1/-2 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 13.6 GPa | 1970 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1013G45 1 NA PA6-GF45 45% Glass Reinforced, Injection Molding |
|||
Tensile Modulus | 13.6 GPa | 1970 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45 45% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 13.6 GPa | 1970 ksi | 1mm/min; ISO 527 |
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |