Mechanical Properties Metric English Comments
Tensile Modulus 13.56 GPa
1967 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA
LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 13.56 GPa
1967 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA (Asia Pacific)
LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.