Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527 |
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527 |
Quadrant EPP Cestilene™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | |
Radici Radilon® A ESL128 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | 1 mm/min |
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527 |
FKuR Kunststoff Terralene® WF 3516 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-4210 10% Chalk-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-4210 is a 10% chalk-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-4210 is developed for producin.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527 |
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance... |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPC 5752 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 5752 is a nucleated controlled-rheology heterophasic copolymer. PPC 5752 is characterized by a high impact resistance and excellent antistatic properties. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPH 7089 Polypropylene Homopolymer, Fiber Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPH 9082 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9082 is a controlled-rheology and antistatic homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing impr.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPM H250 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Total PPC 3640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel.. |
|||
Tensile Modulus | 1.35 GPa @Temperature 23.0 °C |
196 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET
(Unverified Data**) Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | ISO 527-2 |
Domo 2348TC Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 6000IH Nylon Alloy, Flexible Grade (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the covering of.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | 1 mm/min |
Arkema Group Orgalloy® LE 60SF Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).lower in viscosity than LE 6000, adapted to Suited to the cast film.. |
|||
Tensile Modulus | 1.35 GPa | 196 ksi | |
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |