Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.47 GPa | 1954 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS (Asia Pacific) LNP* Thermocomp* CF008 is a compound based on Polystyrene resin containing Glass Fiber. |