Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.350 GPa | 195.8 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436W10L1 Wollastonite Reinforced |
|||
Tensile Modulus | 1.350 GPa | 195.8 ksi | ASTM D638 |
Aclo Accutech TPO TPO030T9V Paintable Grade Approved to Suzuki Spec Black B14257 |