Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-40LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 13.0 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
1890 ksi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2/1 |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC003SXS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC003SXS is a compound based on PA 66 resin containing Carbon fiber. Added features include: Electrically Conductive, Heat Stabilized |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO R 527 |
Solvay TECHNYL® A 118L V50 PA66, 50% glass fiber, Eh 0 Description: TECHNYL A 118L V50 is a polyamide 6.6 reinforced with 50% of glass fiber, with thermal stability, UV protection and modified viscosity that provides better superficial appearance. Color.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50 Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® OCD2100 BK27021 PA46-GF40 40% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 360 S PET-33% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 370 XL PET-GF35 35% Glass Reinforced, Low Outgassing |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527-1/-2 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | ISO 527 |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Conditioned, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
Tensile Modulus | 13.0 - 15.0 GPa | 1890 - 2180 ksi | ISO 527 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | |
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Tensile Modulus | 13.0 GPa | 1890 ksi | |
LATI Latimass 62-05 D040 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |