Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.8 GPa | 1860 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | ASTM D638 |
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | ISO 527 |
Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | |
LATI Laticonther 82 CP1/800 PA12 High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 12.8 GPa | 1860 ksi | |
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered.. |