Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.20 GPa | 174 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | |
LyondellBasell Lupolen® 5261 Z HI HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-3110 TO BU 10% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-3110 TO BU is a 10% talc-filled, black colored and UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3110 TO BU is developed for producing injection mol.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-9000 Polypropylene Block-Copolymer INNOPOL® CS 2-9000 is a polypropylene block-copolymer based compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-9000 is developed for producing injection molded a.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527 |
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® AC 30 000000 Nylon 66 PA 66, injection molding-grade, non-reinforced, higher notched impact strength than A 30 / A 31 in the dry and conditioned stateApplication Examples: plug connectors, cable binders, cable clips, par.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BC 30 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, rapid processing, higher notched impact strength than B 30 S / B 31 SK in dry and conditioned state, impact-modified |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1 mm/min; ISO 527 |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1mm/min; ISO 527-3 |
Borealis Borclear™ RF366MO Polypropylene Random Copolymer for Injection Molding Borclear™ RF366MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleati.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1mm/min; ISO 527-2 |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1mm/min; ISO 527-2 |
Borealis RJ900MO Polypropylene Random Copolymer RJ900MO is a polypropylene random copolymer with high melt flow and good transparency. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and .. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527-1/-2 |
Unitika A1030JR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ASTM D638 |
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6 30% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPC 7712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7712 is a heterophasic copolymer. PPC 7712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early .. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications Bormed RG835MO is specially modified polypropylene random copolymer with high melt flow intended for use in medical and medical related articles. RG835MO is modified with an internal lubricant for .. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ VB4411 TPO Compound Daplen VB4411 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen VB4411 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527-1/-2 |
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 HWUVCP Nylon 6, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | Through Plane Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | cond.; DIN 53 457 |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG53 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C30L1 Calcium Reinforced |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | ISO 527 |
BASF Ultramid® A3K Q603 PA66 (Conditioned) Description: Ultramid A3K Q603 is a general purpose PA6/6.Information provided by BASF |
|||
Tensile Modulus | 1.20 GPa | 174 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |