Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.5 GPa | 1670 ksi | RT; ASTM D638 |
Rogers Corporation XT/duroid™ 8100 0.002" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ASTM D638 |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | dry; ISO 527-1/-2 |
DSM Akulon® S223-PG8 PA66-GF40 40% Glass Reinforced, Impact Modified |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | dry; ISO 527-1/-2 |
DSM Akulon® Ultraflow K-FKGS6 /B PA6-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DSM Arnite® B427 SE/R PBT-GF35 FR(17) 35% Glass Reinforced, Flame Retardant |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-35 PA6-GF35 Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-5H PA12-GF50 Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET) Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON LX04420C PEEK LNP* STAT-KON* LX04420C is a compound based on Polyetheretherketone resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding Syst.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ASTM D638 |
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |