Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accucomp Polyethylene HD0205L High Density |
|||
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized |
|||
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436C10L1 Calcium Reinforced |
|||
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C20L Calcium Reinforced |
|||
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437M10L Mica Reinforced |
|||
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W10L1 Wollastonite Reinforced |
|||
Tensile Modulus | 1.100 GPa | 159.5 ksi | ASTM D638 |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |