Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.16 GPa | 1474 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 10.16 GPa | 1474 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Asia Pacific) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 10.16 GPa | 1474 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Europe-Africa-Middle East) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 10.16 GPa | 1474 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Tensile Modulus | 10.16 GPa | 1474 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |